Laboratory Data --- Typical Properties


| Weight | 1.000000 |
|---|---|
| Data Sheets | |
| Application | For the average-size bathtub (35 square foot surface), mix 10 oz. of Poly Glass 320 resin with 5 oz. of Universal Catalyst (by volume). Thin with 5 oz. of All Purpose Reducer to spray apply. Spray 1 light tack coat followed by 2 wet coats. Pause between coats to inspect the work. Allow the coating to “tack’ before applying the next coat. At 75F and 50% humidity, Poly Glass 320 Resin will dry to touch in approximately eight minutes. Remove masking paper and apply the caulk in 30-45 minutes after the last coat is applied. |